A La/B₄C mirror for 6.7 nm

A 200-bilayer lanthanum/boron-carbide mirror calculated at 6.7 nm: peak reflectivity, the narrow bandwidth, and sensitivity to bilayer count and angle.

EUV Insight · Calculated example · Updated
0%6.55020%6.62540%6.70060%6.77580%6.850Wavelength (nm)
200 La/B₄C bilayers on silicon: 68.9% peak reflectance at 6.700 nm. Reflectance versus wavelength; the dashed line marks 6.7 nm. Normal incidence, unpolarized, smooth interfaces. Calculated, not measured.
Open this design in the app ProRepeated multilayers require Pro.

Why this design

Lanthanum with boron-carbide spacers works just above the boron K absorption edge near 6.6 nm, where boron absorbs least. The index contrast is small, so many more bilayers are needed than at 13.5 nm.

Design inputs

Inputs for the La/B₄C · 6.7 nm example
InputValue
Bilayers200
Period d3.37 nm
Absorber fraction Γ0.4
Absorber1.348 nm La, 6.15 g/cm³
Spacer (on top)2.022 nm B₄C, 2.52 g/cm³
SubstrateSi, 2.33 g/cm³
Wavelength range6.55–6.85 nm, 161 points
IlluminationNormal incidence, unpolarized
InterfacesSmooth (no roughness)

Calculated result

How the peak builds as bilayers are added (normal incidence)
BilayersPeak reflectivity (%)Peak wavelength (nm)FWHM (nm)R at 6.7 nm (%)
5031.116.67510.122229.98
10057.586.69600.078357.35
20068.856.69960.060768.85

Adding bilayers raises the peak and narrows it until absorption in the upper layers stops deeper interfaces from contributing. Past that point, more layers add deposition time and accumulated thickness error without adding reflectance.

The same stack at other incidence angles
Angle from normal (°)Peak reflectivity (%)Peak wavelength (nm)FWHM (nm)R at 6.7 nm (%)
068.856.69960.060868.85
570.716.67610.058145.40
1077.366.62380.05421.53
207.126.27280.07840.22

The peak moves to shorter wavelength as the angle from normal grows, so reflectivity at the fixed design wavelength falls even while the peak itself survives. The angle rows are calculated over a wider wavelength range so the shifted peak stays in view. A mirror used off-normal needs a longer period.

What this model leaves out

The reflectance band is much narrower than a Mo/Si mirror at 13.5 nm (compare the FWHM values), so period errors matter far more. Compound formation at the interfaces lowers the peak in fabricated mirrors and is not part of this model.

The calculation uses bundled reference optical constants and a planar stack. It does not establish mechanical strength, thermal behavior, lifetime or fabrication feasibility.

Next steps

  1. Open the design in the app and confirm the inputs match the table above.
  2. Add interface roughness or a capping layer and compare against the pinned ideal design.
  3. Run a wavelength × angle map over your illumination range, then a thickness-tolerance analysis against your reflectivity requirement.

Calculated with the production solver from the bundled optical reference tables, not measured samples. Example-data fingerprint: 1f022e35fcfc99b7. Assumptions and data sources.